6.6 Subject term (key word) listing.
Capacitance
Vibration
6.7 Tin whisker growth. The use of alloys with a tin content greater than 97 percent, by mass, may exhibit tin
whisker growth problems after manufacture. Tin whiskers may occur anytime from a day to years after manufacturer
and can develop under typical operating conditions, on products that use such materials. Conformal coatings applied
over top of a whisker prone surface will not prevent the formation of tin whiskers. Alloys of 3 percent lead, by mass,
have been shown to inhibit the growth of tin whiskers. For additional information on this matter, refer to ASTM-B545
(Standard Specification for Electrodeposited Coatings of Tin).
6.8 Changes from previous issue. The margins of this specification are marked with asterisks to indicate where
changes from the previous issue were made. This was done as a convenience only and the Government assumes no
liability whatsoever for any inaccuracies in these notations. Bidders and contractors are cautioned to evaluate the
requirements of this document based on the entire content irrespective of the marginal notations and relationship to